Engineered for the perfect bond. Bonolit AAC Thin-Bed Mortar sets the standard for efficiency, reducing material usage while maximizing structural integrity.
Start with a dust-free surface. Measure 6-8 liters of clean water for one 25kg bag.
Pour mortar into water. Mix to remove lumps. Rest for 10 mins, then mix again for consistency.
Apply a thin layer (2-3mm) using a gas concrete trowel. Ensures minimal bridge thermal.
Place block. Adjust with a rubber hammer. Clean spills immediately.
Millimeter sensitivity allows for extremely thin joints, reducing thermal bridges.
Significantly lower material consumption compared to conventional mortar mixes.
Smooth consistency allows for rapid application, speeding up project timelines.
Specifications and Usage Calculation
| Correction Time | ≤ 6 min |
| Workability Time | ≤ 240 min |
| Chloride Content | ≤ 0.1% |
| Air Content | ≤ 20% |
| Compressive Strength | M 10 |
| Dry Density | 94 |
| Thermal Conductivity | 0.49 W/m.K |
Get the complete technical specification sheet or talk to our engineers about your project needs.